System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 60% Glass Fiber Filler
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.
Polypropylene with 60% long glass fiber reinforcement
Information provided by PlastiComp, Inc.
Key Words:
Complet® Long Fiber LGF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.48
g/cc
ASTM D-792
Filler Content
60 %
Long Glass Fiber
Mechanical Properties
Original Value
Comments
Tensile Strength
117
MPa
ASTM D-638
Elongation at Break
1.0 - 2.0 %
ASTM D-638
Tensile Modulus
11034
MPa
ASTM D-638
Flexural Strength
186
MPa
ASTM D-790
Flexural Modulus
10345
MPa
ASTM D-790
Izod Impact, Notched
342
J/m
ASTM D-256
Izod Impact, Unnotched
694
J/m
ASTM D-4812
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
153
°C
ASTM D-648
Processing Properties
Original Value
Comments
Rear Barrel Temperature
390
-
410
°F
Middle Barrel Temperature
400
-
420
°F
Front Barrel Temperature
410
-
430
°F
Nozzle Temperature
400
-
420
°F
Melt Temperature
410
-
430
°F
Mold Temperature
175
°F
Injection Velocity
2.00
-
3.00
in/sec
Drying Temperature
93.0
°C
@Time 7200 sec
Back Pressure
25.0
-
50.0
psi
Cushion
0.250
in
Screw Speed
30
-
50
rpm
Descriptive Properties
Injection Pressure
Medium to maximum
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF
PPLASTI918 / 159329
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.