MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 3181 Polypropylene, Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Low melt flow homopolymer for sheet extrusion, strapping, and thermoforming applications

Melt Strength – The high melt strength of FINA 3181 allows uniform drawdown during processing, resulting in maximum line speeds and a good balance of physical properties.

Process Stability – Excellent polymer stability of FINA 3181 produces consistent product properties during extrusion, even with the use of regrind.

FDA – FINA 3181 complies with all applicable FDA regulations and may be used under these provisions for food contact applications.

Recommended Applications -- FINA 3181 is recommended for sheet extrusion, strapping, and thermoforming applications where high melt strength and high extrusion speeds are required.

Processing – FINA 3181 processes on conventional extrusion equipment with typical melt temperatures of 390-450°F (200-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 0.75 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D288A
Hardness, Shore D 81ASTM D1706
Tensile Strength, Ultimate 34.0 MPaASTM D638
Elongation at Break 8.0 %ASTM D638
Modulus of Elasticity 1.515 GPaASTM D638
Flexural Modulus 1.38 GPaASTM D790
Izod Impact, Notched 0.420 J/cmASTM D256A
Izod Impact, Unnotched 15.9 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 165 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 104 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 232 °CExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom TRC 482N C12628 Polypropylene with 20% Talc Filler
Polykemi AB POLYfill PPC GF2007 PD1 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
INEOS Styrolution PS 168 N/L GPPS
INEOS Styrolution PS 165 N/L GPPS
INEOS Styrolution PS 158 N/L GPPS

PFIN00 / 38330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.