MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology Chloroprene Neoprene Sponge
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Good resistance to heat and moderate chemicals and moderate resistance to oils. Has good characteristics to resist sea water, acids, fats, greases and many solvents. Neoprene has good ozone resistance and flame retardant properties.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.110 - 0.150 g/cc0.110 - 0.150 g/cc
Water Absorption 5.0 %5.0 %
Deformation 25 %
@Pressure 0.0350 - 0.0630 MPa
25 %
@Pressure 5.08 - 9.14 psi
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040base rubber
Tensile Strength 0.450 MPa65.3 psi
Elongation at Break 150 %150 %
Compression Set <= 10 %
@Temperature 23.0 °C,
Time 86400 sec
<= 10 %
@Temperature 73.4 °F,
Time 24.0 hour
50%
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °Fcontinuous
 100 °C212 °Fintermittent
Minimum Service Temperature, Air -34.0 °C-29.2 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Monarch® F-02001 Neoprene Based Rubber Foam
Garlock 244 Neoprene Rubber - Commercial Grade
Polychloroprene Rubber (CR)
3M Scotch-Weld™ 10 Neoprene Contact Adhesive
Armacell Monarch® F-05013 (Black) Neoprene, EPDM, SBR Blend Foam

PPPTEC020 / 133484

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.