MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Sarlink® TPV 4155B03 BLACK Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 4155B03 Black is an engineered thermoplastic vulcanizate material designed primarily for demanding industrial applications, including pipe seals. This product is a medium hardness, low density grade that exhibits excellent compression set, flex fatigue resistance, and medium heat resistance performance. The material can be processed by injection molding, blow molding and extrusion for applications such as seals gaskets, chemical resistant hose and tube, boots and bellows a well a other profiles. It complies with ASTM F477 standard.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Excellent Elastic Recovery; Fatigue Resistant; Good Compression Set; High Melt Stability; Low Density; Low Specific Gravity; Medium Hardness; Medium Heat Resistant

Uses: Automotive Applications; Blow Molding Applications; Gaskets; Hose; Industrial Applications; Pipe Seals; Profiles; Seals: Tubing

Agency Ratings: ASTM F477

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding; Blow Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ISO 1183
Viscosity 306 cP
@Shear Rate 206 1/s,
Temperature 200 °C
306 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  53
@Time 5.00 sec
53
@Time 0.00139 hour
Extruded; ASTM D2240
 57
@Time 5.00 sec
57
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 5.40 MPa783 psiAcross Flow; ASTM D412
 6.10 MPa885 psiFlow; ASTM D412
 5.08 MPa
@Treatment Temp. 70.0 °C,
Time 346000 sec
737 psi
@Treatment Temp. 158 °F,
Time 96.0 hour
After Aging; Flow; ATM D570
Tensile Stress at Strain  1.79 MPa
@Strain 100 %
260 psi
@Strain 100 %
Flow; ASTM D412
 1.83 MPa
@Strain 100 %
266 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 480 %480 %Flow; ASTM D412
 540 %540 %Across Flow; ASTM D412
Compression Set 20 %
@Temperature 70.0 °C,
Time 79200 sec
20 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Processing Temperature 187 - 220 °C369 - 428 °FInjection
Rear Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Middle Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Front Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Nozzle Temperature 187 - 220 °C369 - 428 °FInjection
Zone 1 180 - 200 °C356 - 392 °FExtrusion
Zone 2 180 - 205 °C356 - 401 °FExtrusion
Zone 3 187 - 210 °C369 - 410 °FExtrusion
Zone 4 187 - 210 °C369 - 410 °FExtrusion
Die Temperature 195 - 215 °C383 - 419 °FExtrusion
Melt Temperature 195 - 215 °C383 - 419 °FExtrusion
Mold Temperature 10.0 - 55.0 °C50.0 - 131 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1157 / 237648

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.