MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

TriSteel

(Viewing data as-entered. Click here to return)
TriStar TriSteel PE Metal Backed PTFE Bearing System
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polyethylene (PE)

Material Notes: Ultraflon 603 PE lined metal backed bearing system, with or without lube, high PV, high temperature... Ultraflon 603 PE Liner is a bearing grade polymer for use in lubricated or unlubricated environments. With lubrication, PV ratings can be in excess of 1,000,000. Lubrication reservoirs are available on the liner to produce a constant storage and pumping action for better hydrodynamic film generation. For dry applications reservoirs are not used.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.45 g/cc
Water Absorption 0.15 %
@Time 86400 sec
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 97
Tensile Strength, Yield 32000 psi
Elongation at Break 5.0 %
Flexural Strength 50000 psi
Flexural Modulus 2.00e+6 psi
Compressive Strength 19700 psi
 40000 psiMaximum Static Bearing Load
Compressive Modulus 2.00e+6 psi
Limiting Pressure Velocity 100000 psi-ft/minUnlubricated. Max P = 40,000 psi and max V = 2000 fpm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 28.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 450 °FContinuous
 500 °FShort Term
Brittleness Temperature -100 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TriStar TriSteel AC Metal Backed PTFE Bearing System
TriStar TriSteel PT Metal Backed PTFE Bearing System
TriStar TriSteel AT Metal Backed PTFE Bearing System
TriStar TriSteel PR Metal Backed PTFE Bearing System
DuPont Mobility and Materials Delrin® 100AF POM-PTFE20

PTRIST992 / 176086

TriSteel

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.