System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
AISI 8650 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
Categories:
Metal
;
Ferrous Metal
;
Alloy Steel
;
AISI 8000 Series Steel
;
Low Alloy Steel
;
Carbon Steel
;
Medium Carbon Steel
Material Notes:
Post oil quenched hardness 61 HRC surface, 61 HRC half-radius, 61 HRC center
Key Words:
UNS G86500, ASTM A322, ASTM A505, ASTM A519, SAE J404, SAE J412, SAE J770
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.85
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Brinell
363
Hardness, Knoop
392
Converted from Brinell
Hardness, Rockwell B
100
Converted from Brinell
Hardness, Rockwell C
40
Converted from Brinell
Hardness, Vickers
384
Converted from Brinell
Tensile Strength, Ultimate
1225
MPa
Tensile Strength, Yield
1165
MPa
Elongation at Break
14.6 %
in 50 mm
Modulus of Elasticity
205
GPa
Typical for steel
Bulk Modulus
160
GPa
Typical for steel.
Poissons Ratio
0.29
Calculated
Machinability
60 %
annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus
80.0
GPa
Typical for steel.
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000234
ohm-cm
Typical steel
Thermal Properties
Original Value
Comments
Specific Heat Capacity
0.475
J/g-°C
Typical steel
Thermal Conductivity
46.6
W/m-K
Typical steel
Component Elements Properties
Original Value
Comments
Carbon, C
0.48 - 0.53 %
Chromium, Cr
0.40 - 0.60 %
Iron, Fe
96.54 - 97.67 %
As remainder
Manganese, Mn
0.75 - 1.0 %
Molybdenum, Mo
0.15 - 0.25 %
Nickel, Ni
0.40 - 0.70 %
Phosphorus, P
<= 0.035 %
Silicon, Si
0.15 - 0.30 %
Sulfur, S
<= 0.045 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AISI 4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs.
AISI 6150 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 6150 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 8650 Steel, annealed
AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
M865AG / 8516
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.