MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials GE Sealants & Adhesives Ultra Seal Pro Siliconized Acrylic Latex Caulk, White
Categories: Polymer; Thermoset; Silicone

Material Notes: Ultra Seal Pro Siliconized Acrylic Latex is an advanced grade caulk ideal for decorative and paint projects. Formulated with Bio Seal Antimicrobial Mold-Control, this cured caulk is resistant to stain-causing mold and mildew growth. This formulation offers durable flexibility and excellent adhesion to a wide variety of kitchen and bath materials. It is low in odor, guns out effortlessly, tools smoothly, and cleans-up easily with soap and water. This paint-friendly caulk resists cracking with most latex and oil-based paints. Ultra Seal Pro caulk creates cured seals that are durable enough to withstand frequent cleanings and retain their original fresh look. Guaranteed for as long as you own your home.

Bio-Seal Antimicrobial product protection provides product with excellent resistance to mold & mildew growth. Strong adhesion and flexibility for long lasting results. Waterproof, Paint-Friendly. Durable and scrubbable. Low odor and low VOC (Meets CARB VOC Limits). Easy application. Soap and water clean-up.

Ultra Seal Pro Siliconized Acrylic Latex caulk can be used in a wide variety of interior and exterior applications, including trim, cabinets, walls, molding, tiles, and countertops, showers, sinks and tubs.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0582 lb/in³Uncured
Solids Content 74 - 78 %74 - 78 %Uncured. % by weight; ASTM C1250
Volatile Organic Compounds (VOC) Content <= 33 g/l<= 33 g/lUncured. Excluding water & exempt compounds
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050ASTM 661
Elongation at Break 500 %500 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 100 °C104 - 212 °FApplication Temp
Cure Time 1440 min24.0 hour3/16 inch bead size
Tack-Free Time 40.0 min0.667 hourASTM C679
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceSmooth & CreamyUncured
BaseAcrylic Latex
Carb Chem Curing VOC<1.5 wt.%Uncured. Non-Chem Curing.
Clean-upDamp Disposable Cloth
ColorWhiteMAKB310WT 12C, MAKB305WT 5TG
Consistency / SagPassed
Coverage Rate51 Lin. Ft.
Cracking & CaulkingNone-passedASTM C792
Extension Recovery and Adhesion (Glass/Al.)Passed
Freeze/Thaw StabilityPassed / 5 Cycles at 0°FUncured
Heat Aging and Weight Lost Cracking, CaulkingPassed
Low Temperature FlexibilityPassedASTM C732
OdorSlight AcrylicUncured
Paint Ready Time20 minutes
PaintableLatex & Oil Based Paints
Peel StrengthPassedASTM C794, Dry
Stain/Color ChangePassedASTM C510
Water Ready24 hoursUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9952 / 265765

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.