MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) AmodelĀ® AE-4133 PPA, Conditioned
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: Data for conditioned samples. MatWeb has a more thorough entry for dry samples.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+14 ohm-cm5.00e+14 ohm-cmASTM D257
Dielectric Constant  3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
ASTM D150
 3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 60250
 4.3
@Frequency 60 Hz
4.3
@Frequency 60 Hz
ASTM D150
 4.3
@Frequency 60 Hz
4.3
@Frequency 60 Hz
IEC 60250
Dielectric Strength  19.0 kV/mm
@Thickness 3.20 mm
483 kV/in
@Thickness 0.126 in
ASTM D149
 19.0 kV/mm
@Thickness 3.20 mm
483 kV/in
@Thickness 0.126 in
IEC 60243-1
Dissipation Factor  0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
ASTM D150
 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
IEC 60250
 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
ASTM D150
 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
IEC 60250
Comparative Tracking Index 600 V600 VUL 746
 600 V600 VIEC 60112
High Voltage Arc-Tracking Rate, HVTR 18.0 mm/min0.709 in/minUL 746
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4070 / 279870

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.