MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3HG2 UN00002 Nylon 66, 10% Glass Fiber Reinforced (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Ultramid A3HG2 UN00002 is a 10% glass fiber reinforced injection molding PA66 grade.

Applications: Typical applications include machinery components and housings of medium stiffness, as well as electrically insulating parts.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Moisture Absorption 1.90 - 2.30 %50% RH; ISO 62
Water Absorption at Saturation 6.3 - 7.3 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPaISO 527
Elongation at Break 2.3 %ISO 527
Tensile Modulus 4830 MPaISO 527
Flexural Modulus 4290 MPaISO 178
Izod Impact, Notched (ISO) 4.20 kJ/m²
@Temperature -40.0 °C
ISO 180
 4.20 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact Unnotched 26.0 kJ/m²ISO 179
Charpy Impact, Notched 3.70 kJ/m²
@Temperature -40.0 °C
ISO 179
 4.00 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmIEC 60093
Dielectric Constant 5.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.16
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 235 °CISO 75
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 305 °C
Mold Temperature 45.0 - 105 °Ccan be used where applicable
 80.0 - 90.0 °Crecommended
 80.0 - 90.0 °C
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
Moisture Content <= 0.15 %
Injection Pressure 500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASF8940 / 254898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.