MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 920CX-FM40J-6-42% 125°C Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: High modulus carbon, Unidirectional, 165 g/m2

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1760 MPapr EN 2561 Type B
Tensile Modulus 215 GPaResults normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; pr EN 2561 Type B
Compressive Yield Strength 240 MPaCompression After Impact @ 6.6 J/mm, Results normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; pr EN 6038
 894 MPaResults normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; EFA TP-003
Shear Strength 76.0 MPaIL; pr EN 2563

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ultracor® UKF-68-3/8-2.0 Honeycomb Core Material
Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric
Fibre Glast 2000 / 2020 System 2000 Epoxy
Aremco Aremco-Bond™ 2200 High Performance Epoxide

PHEXC062 / 98532

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.