MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

EOS ToolSteel 1.2709 DMSL on EOS M 290
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Maraging Steel

Material Notes: EOS ToolSteel 1.2709 is an ultra high strength tooling grade maraging steel. Its excellent properties are enabled by forming intermetallic phases and precipitates in heat treatment. The properties enable successful use in diverse applications including injection molding and cold and hot working.

Main Characteristics:

  • Ultra high strength and hardness
  • Properties adjustable with different heat treatment
  • Excellent fatigue strength
  • Good machinability
Typical Applications:
  • Plastic injection molding
  • Extrusion tools
  • Hot pressing tools
  • Die casting tools for aluminum and zinc alloys

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 8.05 g/cc>= 0.291 lb/in³ISO 3369
Particle Size 20 - 65 µm20 - 65 µm
Thickness 40.0 microns1.57 milLayer Thickness
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5757ISO 6508
Tensile Strength 2250 MPa326000 psiHorizontal, Heat Treated State; ISO 6892-1
 2260 MPa328000 psiVertical, Heat Treated State; ISO 6892-1
Tensile Strength, Yield 2170 MPa315000 psiHorizontal, Heat Treated State; ISO 6892-1
 2180 MPa316000 psiVertical, Heat Treated State; ISO 6892-1
Elongation at Break 3.3 %3.3 %Vertical, Heat Treated State; ISO 6892-1
 4.2 %4.2 %Horizontal, Heat Treated State; ISO 6892-1
Fatigue Strength 732 MPa
@# of Cycles 1.00e+7
106000 psi
@# of Cycles 1.00e+7
ASTM E466
Charpy Impact 10.0 J7.38 ft-lbV-notch; ISO 148-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.72 µm/m-°C
@Temperature 25.0 - 100 °C
5.956 µin/in-°F
@Temperature 77.0 - 212 °F
ASTM E228
 11.15 µm/m-°C
@Temperature 25.0 - 200 °C
6.194 µin/in-°F
@Temperature 77.0 - 392 °F
ASTM E228
 11.5 µm/m-°C
@Temperature 25.0 - 300 °C
6.39 µin/in-°F
@Temperature 77.0 - 572 °F
ASTM E228
 11.51 µm/m-°C
@Temperature 25.0 - 400 °C
6.394 µin/in-°F
@Temperature 77.0 - 752 °F
ASTM E228
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 8.5 - 10 %8.5 - 10 %
Iron, Fe 64.6 - 69.2 %64.6 - 69.2 %Balance
Molybdenum, Mo 4.5 - 5.2 %4.5 - 5.2 %
Nickel, Ni 17 - 19 %17 - 19 %
Titanium, Ti 0.80 - 1.2 %0.80 - 1.2 %
 
Descriptive Properties
Volume rate4.1 mm3/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS971 / 280631

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.