MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LKAB Minerals Aggregates
Categories: Ceramic

Material Notes: Marble is a form of calcium carbonate. Dolomite is magnesium calcium carbonate.

Italian Marble colors include Black, Botticino, Breccia Aurora, Red Verona, Rosa Corallo, Verdi Alpi, White and Yellow Sienna.
Spanish Marble colors include Beige and Grey.
White Dolomite is available from Greek and Spanish sources. Applications: White and colored grades are used in a number of bulk applications including concrete production, garden landscaping and flooring applications. colored grades are particularly useful for achieving decorative effects in building cladding panels, terrazzo floor tiles, seamless flooring and any building application where color adds aesthetic appeal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
AppearanceGranular particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Accuratus MACOR Machinable Glass Ceramic
Bostik D-2001® Ultra-Premium™ Ceramic Tile Mastic
Bostik Big Tile & Stone™ Latex-Modified Mortar
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Bostik Glass-Mate™ Glass Tile Mortar

CMINEL09 / 1574

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.