MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® L5040TC High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Applications
ALATHON L 5040TC is a bimodal high density polyethylene copolymer natural resin designed for telecommunications conduits. L 5040TC offers an excellent balance of stiffness, toughness and ease of processing. This resin is ideal for conduit used with fiber optic cable, electrical cable and telecommunications cable.

Regulatory Status
L 5040TC meets the requirements of D 3350 cell classification 335440A. Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing L 5040TC can only be made when the processing conditions, equipment and end use are known.
Cell Classification 335440A, ASTM D3350.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³ASTM D1505
ESCR 100% Igepal® >= 1000 hour>= 1000 hourF50; ASTM D1693
Melt Flow 0.40 g/10 min0.40 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength, Yield 23.4 MPa3400 psiASTM D638
Elongation at Break >= 600 %>= 600 %ASTM D638
Flexural Modulus 1.10 GPa160 ksiASTM D790
Tensile Impact 100 J/cm188 ft-lb/inASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C169 °FASTM D648
Vicat Softening Point 128 °C262 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5332CP High Density Polyethylene
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade
JPJ Technologies 7600M HDPE Extrusion
LyondellBasell Alathon L 4930TC High Denisty Polyethylene
LyondellBasell Alathon® L5008 High Density Polyethylene

PEQU0578 / 37048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.