MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam
Categories: Polymer; Thermoplastic

Material Notes: HYTAC®-XTL was developed to offer an improved surface quality after machining when compared to our popular HYTAC-B1X. This is particularly important when working with sticky or transparent plastics due to the challenge of polishing any thermoplastic syntactic material.

Thermoplastic syntactic foams from CMT have become a good choice for plug assist due to their low thermal conductivity and ability to withstand chips and dings associated with any typical thermoforming process.

In addition to enhanced surface quality, HYTAC-XTL has these outstanding attributes:

  • The highest toughness ratings for any syntactic foam
  • Good machinability with no dust
  • Excellent where edge definition and detail are required
  • Low thermal conductivity
  • Low coefficient of thermal expansion
  • Excellent material distribution

Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet specific needs.

Applications: HYTAC-XTL is the first material to combine the machined surface quality of an epoxy syntactic with the durability and dust free machining of a thermoplastic syntactic foam. Excellent surface characteristics optimize material distribution with most plastics.

Recommended for use with PP, PET, PE, APET, CPET, HIPS, OPS, PETG, PLA, PS, PVC and RPET

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 45.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Flexural Toughness 23.0 psiASTM D790
Compressive Strength 10220 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µin/in-°F
Thermal Conductivity 0.170 W/m-K
Maximum Service Temperature, Air 350 °F
 
Descriptive Properties
ColorMauve

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Pocan® B 1505 000000 PBT
CMT Materials HYTAC® B1X High Durability Thermoplastic Syntactic
CMT Materials HYTAC® B Solid Polymer Tooling Material
CMT Materials HYTAC® FLXT High Temperature, PTFE Impregnated Copolymer Syntactic
Mitsubishi Chemical Advanced Materials Nylatron™ MC 901 H.S. PA6

PCMT008 / 146232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.