MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt S 122 LS Putty
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: S 122 LS series is a white low density, slightly thixotropic and low viscosity polyester-based compound that gels and cures @ room temperature by adding methyl ethyl ketone peroxide catalyst. The intended use for this putty is to serve as a gap filling and laminating material in a “Squish Molding” process. S122LS series serves also to bond to the skin of double sided panels and parts. Components made in this manner produce excellent surface quality on both faces of the specific part. S 122 LS series is an excellent choice for double sided door panels, RV, truck and train panels, satellite dishes, shower bases and marine components such as hatches.

Features And Benefits:

  • S 122 LS has a very low shrink.
  • High bond strength adhesive for laminates.
  • May be pumped with conventional equipment without volume loss.
  • Formulated to use with a MEKP catalyst made of methylethylketone peroxide.
  • Available in 20 liters pails and 205 liters drums.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.730 - 0.760 g/cc
Brookfield Viscosity 4500 - 5500 cPHAF T-A @ 5 rpm
 
Processing PropertiesOriginal ValueComments
Gel Time 55.0 - 75.0 min
@Temperature 25.0 °C
tested @ 77°F (25°C) with 1,5% Norox MEKP-9 in a 100 g mass.
Shelf Life 1.50 Month
 
Descriptive Properties
Peak Exotherm<150°C
Thixotropic Index2-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9019 / 231614

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.