Product Description: A hard, black thermoplastic vulcanizate, TPV (EPDM/PP) in the thermoplastic elastomer family designed for injection applications. The Bondable to: PP, EVA, PE Availability: Africa & Middle East; Asia Pacific; Europe; North America Features: Bondability; High Hardness RoHS Compliance: RoHS Compliant Appearance: Black Forms: Pellets Processing Method: Injection MoldingInformation provided by Elastron |