MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin PKN4775F Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL PKN4775F resin is a non-reinforced, opaque blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS) and is FDA food compliant in several colors. This high heat, thin wall extrusion and injection moldable grade is an improved version of NORYL PKN4775F resin and exhibits modulus at elevated temperature and good chemical resistance. NORYL PKN4775F resin is an excellent candidate for applications in high performance packaging. *See NORYL PKN4775 resin for NON FDA food compliant version.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Thin Wall,Low Warpage,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Density 1.05 g/ccISO 1183
Moisture Absorption 0.000 %Sheet Extrusion
 0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %ISO 62-1
Viscosity 14 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 15.3 g/10 min
@Load 5.00 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 47.0 MPa50 mm/min; ASTM D638
 47.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 51.0 MPa50 mm/min; ASTM D638
 51.0 MPa50 mm/min; ISO 527
Elongation at Break 29.4 %50 mm/min; ISO 527
 35 %50 mm/min; ASTM D638
Elongation at Yield 4.2 %50 mm/min; ISO 527
 5.1 %50 mm/min; ASTM D638
Tensile Modulus 2120 MPa5 mm/min; ASTM D638
 2120 MPa1 mm/min; ISO 527
Flexural Strength 78.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 82.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2160 MPa2 mm/min; ISO 178
 2210 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 268 JASTM D256
 161 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 19.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 39.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 92.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 92.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 122 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 142 °CRate B/50; ASTM D1525
 142 °CRate B/50; ISO 306
 144 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Zone 1 205 - 225 °CSheet Extrusion
Zone 2 215 - 240 °CSheet Extrusion
Zone 3 240 - 265 °CSheet Extrusion
Zone 4 240 - 265 °CSheet Extrusion
Adapter Temperature 240 - 265 °CSheet Extrusion
Die Temperature 240 - 265 °CSheet Extrusion
Melt Temperature 265 - 275 °CSheet Extrusion
Roll Temperature 105 - 120 °CRoll Stack Temp - Bottom
 105 - 120 °CRoll Stack Temp - Middle
 105 - 120 °CRoll Stack Temp - Top
Drying Temperature 70.0 - 80.0 °CSheet Extrusion
Dry Time 2.00 - 4.00 hourSheet Extrusion
 8.00 hourCumulative; Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82421 / 290368

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.