MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haysite 42000 Polyester SMC, 22% Glass Reinforced
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: The 42000 series sheet molding compound is an electrical grade designed for compression molded parts requiring high strength and good electrical properties. This material possesses excellent moldability and is recognized by UL with a 94V-0 flame rating at .060" wall thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/ccASTM D572
Water Absorption 0.18 %ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 69.0 MPa
Flexural Strength 172 MPa
Compressive Strength 193 MPa
Izod Impact, Notched 9.90 J/cmedgewise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.4
@Frequency 60 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmPerpendicular (ASTM D149), Short Time
Dissipation Factor 0.0096
@Frequency 60 Hz
ASTM D150
Arc Resistance 180 secASTM D495
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °Ctemperature rating
Flammability, UL94 V-0File No.E-27875

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haysite 43000 Polyester SMC, 22% Glass Reinforced
Haysite 42100 Polyester SMC, 22% Glass Reinforced
Haysite 46000 Polyester SMC, 30% Glass Reinforced
Applied Composites 150 Polyester SMC
Applied Composites 179 Polyester SMC

PHAY07 / 45613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.