MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Eastman Kristalex™ 5140SD Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Kristalex™ 5140SD hydrocarbon resin is a high softening point, low molecular weight resin with low organic volatile content and low odor, produced by copolymerization of pure aromatic monomers. It is designed primarily for use as a modifier resin in high performance adhesives and coating compositions. In these applications, its water clear color, heat stability, and resistance to oxidation and discoloration are the advantages. In EVA-based hot melt adhesives, Kristalex™ 5140SD is compatible with EVA grades with up to 18% vinyl acetate and is useful in formulating low-color adhesives with improved high temperature resistance. In styrenic block copolymer based adhesives, Kristalex™ 5140SD preferentially associates with the styrenic endblocks, producing higher cohesion at temperatures up to 70°C without affecting tack and adhesion properties. Kristalex™ 5140SD complies with many FDA regulations for applications involving food contact. Users of this product should determine its compliance for their specific application prior to use.

Application/Uses:

  • Alluminum-pigment preparations
  • Assembly
  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
Key Attributes:
  • Excellent thermal stability
  • High softening point
  • Low odor
  • Low organic volatile content
  • Made from purified aromatic monomers
  • Suitable for use in food contact applications
  • Water-white initial color

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cP
@Temperature 220 °C
Melt
 10000 cP
@Temperature 180 °C
Melt
 100000 cP
@Temperature 160 °C
Melt
Molecular Weight 1650 g/molMz
 4650 g/molMw. Mw/Mn ratio = 2.8
 8950 g/molMn
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 90.0 °C
Ring & Ball Softening Point 140 °CASTM E 28
 
Descriptive Properties
Cloud Point>180°COMS
 10°CMMAP
 -40°CDACP
ColorYID

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5341 / 222535

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.