MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

EMS-Grivory Grilamid® XE 4129 black 9020 PA610
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Product description: Grilamid XE 4129 black 9020 is a high viscosity Polyamide 610 especially suitable for extrusion applications. A characteristic of tubes made out of this material is the high resistance to collapse under the influence of vacuum and high temperatures. PA610 polymer is to a large extent based on renewable raw materials and its eco-profile is very favourable when compared to similar products based on crude oil. The main features of Grilamid XE 4129 black 9020 are:
  • high flexibility and impact resistance at low temperatures
  • high stiffness at high temperatures
  • high heat and chemical resistance
  • easy processing
Grilamid XE 4129 black 9020 can be processed on standard tube extrusion lines suitable for polyamides.

Application examples: Grilamid XE 4129 black 9020 was developed for automotive tubing subject to high continuous use and peak temperatures. The material is particularly indicated for brake booster vacuum lines of passenger cars.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³Dry; ISO 1183
Water Absorption 4.1 %4.1 %Sim. to ISO 62
Moisture Absorption 1.50 %1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.016 cm/cm0.016 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 50.0 MPa7250 psiConditioned; ISO 2039-1
 105 MPa15200 psiDry; ISO 2039-1
Tensile Strength at Break 35.0 MPa5080 psiConditioned; ISO 527-1/-2
 40.0 MPa5800 psiDry; ISO 527-1/-2
Tensile Strength, Yield 45.0 MPa6530 psiDry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Conditioned; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %Dry; ISO 527-1/-2
Tensile Modulus 0.700 GPa102 ksiConditioned; ISO 527-1/-2
 1.70 GPa247 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 2.10 J/cm²
@Temperature -30.0 °C
9.99 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+11 ohm-cm1.00e+11 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mm813 kV/inConditioned; IEC 60243-1
 33.0 kV/mm838 kV/inDry; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 150 µm/m-°C83.3 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°C83.3 µin/in-°FISO 11359-1/-2
Melting Point 220 °C428 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 160 °C320 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Hydraulic systems
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
ProcessingOther Extrusion
Product AttributesBio based Polyamide
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® XE 3841 nat PA12
EMS-Grivory Grilamid® LC-15H black PA12-CF15
Evonik Vestamid® Terra HS 22 natural color Nylon 610
Evonik Vestamid® Terra HS 18 natural color Nylon 610
Evonik Vestamid® Terra HS 16 natural Nylon 610

PGRH137 / 156846

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.