MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zylog Hipolyene® 9011 UHF Thermoplastic Polyolefin & PP Compound
Categories: Polymer; Thermoplastic; Polyolefin; Polypropylene (PP)

Material Notes:

Information provided by Zylog Plastalloys Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/cc
Melt Flow 26 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 270 kg(f)/cm²
Elongation at Break 25 %
Flexural Modulus 19000 kg(f)/cm²
Izod Impact, Notched 5.50 kg-cm/cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zylog Hipolyene® 1533 NM Thermoplastic Polyolefin & PP Compound
Zylog Hipolyene® 5198 FLM Thermoplastic Polyolefin & PP Compound
Zylog Hipolyene® 1532 HC EX Thermoplastic Polyolefin & PP Compound
Zylog Hipolyene® 1535 T5 Thermoplastic Polyolefin & PP Compound
Zylog Hipolyene® 8021 HC Thermoplastic Polyolefin & PP Compound

PZYLOG944 / 157260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.