MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyrocks Chemical 168B Polypropylene, halogen-free flame retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: 168B is flame retardant polypropylene with bromine and antimony as the flame retardant elements. Through gas-phase mechanism play the flame retardant performance. 168B flammability can reach UL 94 V-2(1.5mm and 3.0mm),glow-wire test meets GWIT:775/3.0 and GWFI:850/3.0? 168B has characteristics of good flowability?strong chemical resistance?good mechanical properties...etc.

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D792
Linear Mold Shrinkage 0.014 - 0.018 cm/cmASTM D955-08
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 35.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Flexural Strength 40.0 MPaASTM D790
Flexural Modulus 1400 MPaASTM D790
Izod Impact, Notched 35.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-2
@Thickness 1.50 mm
 V-2
@Thickness 3.00 mm
Glow Wire Ignition Temperature 775 °C
@Thickness 3.00 mm
Pass; IEC 60695-2-13
Glow Wire Flammability Index 850 °C
@Thickness 3.00 mm
Pass; IEC 60695-2-13
 
Descriptive Properties
Ball Pressure1.75-1.90 mmIEC 60695-10-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROCKS010 / 278518

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.