MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21TPLV Two Component Epoxy System  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Polysulfide Sealant/Adhesive

Material Notes: EP21TPLV-NV complies with RoHS3 Directive (EU) 2015/863. It is a new version of EP21TPLV, which has been discontinued.

Key Features:

  • One to one mix ratio
  • Flexible bonds
  • Withstands thermal cycling
  • Exceptional chemical resistance to fuels and oils
  • Excellent electrical insulation properties
  • Two part polysulfide system
Product Description: Master Bond EP21TPLV is a two component epoxy polysulfide system formulated to cure at room temperature or more rapidly at elevated temperatures, with a one to one mix ratio by weight or volume. It’s a versatile material that can be used as an adhesive, coating, encapsulant and especially as a sealant. It resists a wide array of chemicals including water, gasoline, fuels, oils, hydrocarbons, hydraulic fluids and many acids and bases. Significantly, unlike many chemical resistant epoxy based materials, this system has excellent toughness. These properties enable EP21TPLV to withstand rigorous thermal cycling as well as mechanical and thermal shocks. It bonds well to a variety of substrates, including metals, glass, ceramics and many rubber and plastic materials. The cured system has excellent electrical insulation properties. Its service temperature range is -80°F to +250°F. One unusual feature of EP21TPLV is the influence of adding heat to the curing cycle. When cured at room temperature the Shore D hardness is 60-65; when cured at 200°F for 2-3 hours, its hardness is 15-20 Shore D. Therefore, to obtain the optimum properties, EP21TPLV should be cured at room temperature. The color of Part A is tan and Part B is amber, although, other colors are available. Polysulfide systems, such as EP21TPLV, have been used as fuel tank sealants and coatings, as well as for potting electrical connectors and other components exposed to fuels, oils and lubricants. EP21TPLV can be used in aerospace, OEM, electronic, electrical, chemical and related industries where room temperature curing, toughness and resistance to fuels, lubricants and similar type chemicals are needed.

Product Advantages:

  • Convenient mixing: forgiving one to one mix ratio by weight or volume
  • Easy to apply — adhesive spreads evenly and smoothly
  • Ambient temperature curing imparts optimal chemical resistance and hardness
  • Produces tough bonds; resistant to thermal cycling
  • Bonds well to similar and dissimilar substrates
  • Superb resistance to oils, fuels and related chemicals

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 50 - 200 cPPart B
 3000 - 4000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60 - 65
Tensile Strength >= 7000 psi
Elongation at Break >= 20 %
Tensile Modulus 150000 - 200000 psi
Adhesive Bond Strength >= 1500 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Constant 4.1
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 - 60.0 µm/m-°C
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -80.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 48.0 - 72.0 hour
Working Life 30.0 - 60.0 minAfter mixing, 100 g batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Mixing Ratio1:1 by weight or volumeParts A to B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant
Master Bond EP21TPND Two Component Polysulfide Epoxy Adhesive
3M AC-250 A-1/6 Aerospace Sealant
Abatron AboSeal 8104-9 Polysulfide, Thixotropic or Self-Leveling Sealant and Caulk
Abatron AboSeal 8104-8 Polysulfide, Thixotropic Sealant and Caulk

PMASTM842 / 185435

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.