MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tritan™ TX1000 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan copolyester's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning detergents.

Application/Uses

  • Appliances
  • Consumer and durable goods
  • Housewares
  • Small appliances

Key Attributes

  • Ease of processing
  • Excellent clarity
  • Excellent hydrolytic stability
  • Fast drying times
  • Good chemical resistance
  • Good heat resistance
  • Outstanding impact resistance
  • Quick cycle times

Typical properties as listed are from preliminary data. Information was provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength at Break 53.0 MPaASTM D638
Tensile Strength, Yield 43.0 MPaASTM D638
Elongation at Break 210 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 1550 MPaASTM D638
Flexural Yield Strength 62.0 MPaASTM D790
Flexural Modulus 1550 MPaASTM D790
Izod Impact, Notched 980 J/mASTM D256
Izod Impact, Unnotched NBASTM D4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Transmission, Visible 90 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 282 °C
Mold Temperature 38.0 - 66.0 °C
Drying Temperature 88.0 °C
Dry Time 4 - 6 hour
 
Compliance PropertiesOriginal ValueComments
FDA YesRepeated use food contact articles
NSF YesFood equipment materials; NSF/ANSI Standard 51

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tritan™ TX2000 Copolyester
Eastman Tritan™ TX1001 Copolyester
Eastman Tritan™ TX1500HF Copolyester
Eastman Tritan™ TX2001 Copolyester
Eastman Tritan™ TX1501HF Copolyester

PE8918 / 109260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.