Beta-Tricalcium phosphate; beta TCP; TCP; Bioceramic materialApplication: Widely used in orthopedic bone substitute and repair materials, plastic surgery and cosmetic surgery, dentistry, etc. Morphology: White strip or column |
Synonyms: Beta-Tricalcium phosphate; beta TCP; TCP |