MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexPly® M92 Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M92 combines all the key benefits achieved individually with other 125ºC curing epoxy resins, in one new system with no compromise: very good hot-wet performance, high toughness, self-adhesion, fire resistance and long out/tack life. This multi-tasking system has elevated hot wet Tg performance, allowing HexPly® M92 to operate at higher service temperatures, while still benefiting from the lower cost 125ºC cure. HexPly® M92 is available in a wide range of prepreg forms (woven and UD tape).

Benefits and Features

  • HexPly® M92 exceeds the service temperature and hot wet retention of standard 125°C curing systems (Tg dry 160°C and Tg wet 115°C measured by DMA)
  • Optimized for sandwich and monolithic structures with self-adhesive properties
  • High toughness suitable for demanding aerospace structures
  • Low exotherm for thick components
  • Fire resistant performance (FAR 25.853 12s and 60s vertical burn test)
  • High robustness with 60 days tack life and out life
  • Low pressure molding capability 0.8-3 bar
  • Good surface aspect - limited preparation before painting

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³
Viscosity  10000 cP
@Temperature 115 °C
10000 cP
@Temperature 239 °F
2°C/min
 200000 cP
@Temperature 60.0 °C
200000 cP
@Temperature 140 °F
2°C/min
 5.00e+8 cP
@Temperature 130 °C
5.00e+8 cP
@Temperature 266 °F
2°C/min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa8700 psiISO R527 type 1
Elongation at Break 2.45 %2.45 %ISO R527 type 1
Tensile Modulus 2.70 GPa392 ksiISO R527 type 1
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9174 / 322330

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.