MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Novarex® 7022E TW3 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Clear. Anti-static grade. Used in a wide range of industries, including sports equipment, medical equipment, automobiles, optics, machinery, office automation equipment, and electronics, they have a reputation for reliability with users. Superior impact strength, Superior transparency. Usability in a wide range of temperatures: -40degC to 120degC.Excellent precision molding properties and dimensional stability. Superior self-extinguishing properties. Excellent weather resistance. Excellent electrical insulation capabilities.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Water Absorption 0.24 %
@Temperature 23.0 °C,
Time 86400 sec
Immersion
Linear Mold Shrinkage, Flow 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
Melt Flow 29 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min Volumetric Rate
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 64.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 6.3 %
Tensile Modulus 2700 MPa
Flexural Strength 101 MPa
Flexural Modulus 2500 MPa
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Charpy Impact, Notched 7.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 3.00e+14 ohm
Dielectric Constant 3.2
@Frequency 100 Hz
 3.2
@Frequency 1e+6 Hz
Dielectric Strength 18.0 kV/mm
Dissipation Factor 0.0017
@Frequency 100 Hz
 0.0097
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
CTE, linear, Transverse to Flow 66.0 µm/m-°C
Maximum Service Temperature, Air 120 °C
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
Deflection Temperature at 1.8 MPa (264 psi) 114 °C
Minimum Service Temperature, Air -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Flint Hills P4G3Z-039 Homopolymer Polypropylene
Flint Hills H0500HN Polypropylene Homopolymer
GEHR Plastics ECO-GEHR® PA 6.10 Nylon 6.10 Dry, 60% Sebacic Acid
INEOS Styrolution Luran® S 797 S UV White 33999 Q455 ASA
INEOS Styrolution Luran® S 797S White 35962 ASA

PMITSU9352 / 192016

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.