MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Torlon® 4630 PAI, Excellent wear resistance in dry environments
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Graphite Filled

Material Notes: Excellent wear resistance in dry environments, contains PTFE and graphite

Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep and chemicals.

Potential applications for Torlon® 4630 polyamide-imide include thrust washers, seal rings, sliding vanes, bobbins, bushings, clutch rollers and pistons.

Applications: Automotive Applications; Bearings; Bushings

Features: Chemical Resistant; Creep Resistant; Flame Retardant; High Heat Resistance; High Stiffness; High Temperature Strength; Low Friction; Wear Resistant

Injection notes: Minimum drying times are: 3 hours at 350°F (177°C), 4 hours at 300°F (149°C), or 16 hours at 250°F (121°C).
Compression Ratio between 1:1 and 1.5:1
Begin hold pressure at a high setting 6,000-8,000 psi (41.37-55.16 MPa), for several seconds, then drop off to 3,000-5,000 psi (20.69-34.48 MPa), for the duration of the hold pressure sequence.
Molded parts must be post cured.

Information provided by Solvay Specialty Polymers.

Vendors: Drake Plastics Ltd. Co. The Torlon Specialist, manufactures & stocks the most complete line of Torlon PAI in machinable rod, plate & Seamless Tube®. Drake works closely with Solvay Specialty Polymers to identify & serve a multitude of new applications. Drake, a lean producer of extruded, injection molded & machined shapes & parts, offers low minimums & quick, economical delivery globally.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccASTM D792
Water Absorption 0.18 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 81.4 MPaASTM D638
Elongation at Break 1.9 %ASTM D638
Tensile Modulus 7450 MPaASTM D638
Flexural Strength 131 MPaASTM D790
Flexural Modulus 6830 MPaASTM D790
Compressive Strength 99.3 MPaASTM D695
Izod Impact, Notched 48.0 J/mASTM D256
Izod Impact, Unnotched 160 J/mASTM D256
K (wear) Factor 1.00 x 10-10 in³-min/ft-lb-hrASTM D3702
 
Thermal PropertiesOriginal ValueComments
CTE, linear 36.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 279 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 304 °C
Nozzle Temperature 371 °C
Mold Temperature 199 - 216 °C
Drying Temperature 177 °C
@Time 10800 sec
Moisture Content <= 0.050 %Injection
Back Pressure 6.89 MPa
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AdditivePTFE + Graphite Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
Screw L/D Ratio, Injection18.0:1.0 to 24.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4549 / 280349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.