MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow SE BR-1203H Stereospecific high cis-1,4 Polybutadiene (BR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SE BR-1203H is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production process. BR-1203H is suitable for tires, conveyor belting, footwear and mechanical goods. It offers a unique property combination of good abrasion resistance, particularly at high severity, excellent groove crack resistance and good heat aging.

Other features include high resilience, low hysteresis, good set properties and a low glass transition point which results in better low temperature performance. BR-1203H is able to accept high filler and oil loadings without significant loss of properties. It may be blended with natural rubber and styrene butadiene (SBR), isoprene (IR), nitrile (NBR), or polychloroprene (CR) synthetic rubbers. BR-1203H is supplied in bales weighing ca. 34 kg. Bales are wrapped in 50 micron PE or EVA film.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 6.4
@Temperature 160 °C
[min]; ts1, (1 RAD); ASTM D2084
 10
@Temperature 160 °C
[min]; T50, (1 RAD); ASTM D2084
 10.8
@Temperature 160 °C
[dNm]; ML, (1 RAD); ASTM D2084
 13.1
@Temperature 160 °C
[min]; T90, (1 RAD); ASTM D2084
 42
@Temperature 160 °C
[dNm]; MH, (1 RAD); ASTM D2084
Mooney Viscosity 48
@Temperature 100 °C
[MU]; ML 1+4; ASTM D1646
Ash 0.030 %ASTM D1416
Collected Volatile Condensable Material 0.20 %ASTM D1416
Storage Temperature <= 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 16.8 MPaDie C (35 min / 145°C); ASTM D412
Tensile Stress at Strain 9.30 MPa
@Strain 300 %
ASTM D412
Elongation at Break 490 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Month
 
Descriptive Properties
Accelerator (TBBS) wt%0.9ASTM D3189
Carbon Black wt%60ASTM D3189; IRB 6
Cis-1,4 Content %97Supplier Method (NMR)
Dry Gel Content mg/kg200Supplier Method
Naphthenic oil type 103 wt%15ASTM D226
Stearic Acid wt%2ASTM D3189
Sulfur content, %1.5ASTM D3189
Zinc Oxide wt%3ASTM D3189

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BCP 817 Stereospecific high cis-1,4 Polybutadiene (BR)
Nitriflex SB-1011 Styrene Butadiene Copolymer
Nitriflex SB-1011G Styrene Butadiene Copolymer
Armacell Monarch® F-05031 (Black) Neoprene, EPDM, SBR Blend Foam

PDOW1097 / 30301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.