MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® 1SBVX-30H LDS black PA1010-GF30
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring technology of LPKF (LPKF-LDS®). The product enables selective planting and creation of electric/electronic circuits or antennas on 3D injection-molded carriers. Key properties of Grilamid 1SBVX-50H LDS black:
  • Suited for Laser Direct Structuring (LDS)
  • High stiffness and strength combined with high toughness
  • Low moisture adsorption
  • High dimensional stability
  • Easy processing
  • Excellent surface finish
  • Outstanding chemical resistance
  • Paintable
  • Polymer primarily based on renewable resources
Applications: Grilamid 1SBVX-30H LDS black is suitable for thin-walled housings/parts with integrated electrical and mechanical functions found mainly in areas such as telecommunication, electro/electronics or automotive.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccDry; ISO 1183
Water Absorption 2.3 %Sim. to ISO 62
Moisture Absorption 1.10 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 150 MPaConditioned; ISO 2039-1
 170 MPaDry; ISO 2039-1
Tensile Strength at Break 110 MPaConditioned; ISO 527-1/-2
 115 MPaDry; ISO 527-1/-2
Elongation at Break 2.0 %Dry; ISO 527-1/-2
 2.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 10000 MPaConditioned; ISO 527-1/-2
 11000 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 40.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 40.0 kV/mmDry; IEC 60243-1
 40.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°CISO 11359-1/-2
Melting Point 200 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °CLong Term; ISO 2578
 150 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 165 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 110 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Powertrain and Chassis
Electricals & ElectronicsMobile phones and other portable devices
FormGranules
Industry & Consumer goodsMedical devices
ProcessingInjection Molding
Product AttributesBio based Polyamide
 Improved flowability and demolding
Special CharacteristicsHigh impact or impact modified
 Platable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
BASF Capron® 8200 HS BK-102 Nylon 6 (Dry)
EMS-Grivory Grilamid® TR 30 LS nat PA*
E-Polymers EFLEX® S1030 General
304 Stainless Steel

PGRH002 / 156711

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.