Georgia Gulf 9275J Amber 05 is used for injection blow molded packages in cosmetic and toiletry applications. It is a pre-colored amber compound and all ingredients are FDA approved. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |