MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gougeon Brothers PRO-SET® HTP 180/HTP 280 High-Temp Laminating Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: High-temperature, high-performance epoxy formulation for synthetic composite part and tooling manufacture.
Tg as high as 300°F (149°C) with proper post cure providing excellent temperature stability and great part cosmetics.
Slow cure speed hardener provides 5 to 6 hours of working time at 72°F (22°C). a typical laminate will gel in 10 to 12 hours at room temperature.
This combination is specifically formulated for resin infusion and VARTM processes. Not for use in open mold applications. Elevated temperature cure is required. Parts can be pulled after 24-48 hours at room temperature or sooner after a mild initial cure of 90-100°F (32-43°C).
Quality-control tinting is available at no extra charge; simply add "QC" after the product code on your order.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³Hardener
 1.15 g/cc0.0415 lb/in³Cured
 1.16 g/cc0.0419 lb/in³Resin
Viscosity  35 cP
@Temperature 22.0 °C
35 cP
@Temperature 71.6 °F
hardener; ASTM D2196
 120 cP
@Temperature 48.9 °C
120 cP
@Temperature 120 °F
Mixed
 380 cP
@Temperature 29.4 °C
380 cP
@Temperature 84.9 °F
Mixed
 600 cP
@Temperature 29.0 °C
600 cP
@Temperature 84.2 °F
Mixed; ASTM D2196
 1300 cP
@Temperature 15.6 °C
1300 cP
@Temperature 60.1 °F
Mixed
 2500 cP
@Temperature 22.0 °C
2500 cP
@Temperature 71.6 °F
resin; ASTM D2196
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9494RT + 60°C x 2hr + 135°C x 12hr; ASTM D2240
Tensile Strength 74.5 MPa10800 psiRT + 60°C x 2hr + 135°C x 12hr; ASTM D638
Elongation at Break 5.5 %5.5 %RT + 60°C x 2hr + 135°C x 12hr; ASTM D638
Tensile Modulus 2.99 GPa434 ksiRT + 60°C x 2hr + 135°C x 12hr; ASTM D638
Flexural Strength 123 MPa17800 psiRT + 60°C x 2hr + 135°C x 12hr; ASTM D790
Flexural Modulus 2.85 GPa414 ksiRT + 60°C x 2hr + 135°C x 12hr; ASTM D790
Compressive Yield Strength 105 MPa15300 psiRT + 60°C x 2hr + 135°C x 12hr; ASTM D695
 
Thermal PropertiesMetricEnglishComments
CTE, linear  53.57 µm/m-°C
@Temperature -30.0 - 30.0 °C
29.76 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM E831
 79.66 µm/m-°C
@Temperature 30.0 - 120 °C
44.26 µin/in-°F
@Temperature 86.0 - 248 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 139 °C282 °FRT + 60°C x 2hr + 135°C x 12hr; ASTM D648
Glass Transition Temp, Tg 151 °C304 °FRT + 60°C x 2hr + 135°C x 12hr, DMA Onset Storage Modulus, 1 Hz, 3°C per minute; ASTM E1640
 151 °C304 °FRT + 60°C x 2hr + 135°C x 12hr, DSC Onset– 1st Heat; ASTM E1356
 160 °C320 °FRT + 60°C x 2hr + 135°C x 12hr, DMA Peak Tan Delta, 1 Hz, 3°C per minute; ASTM E1640
 
Processing PropertiesMetricEnglishComments
Cure Time 600 - 720 min10.0 - 12.0 hourtypical laminate will be gelled
Pot Life  120 min
@Load 0.500 kg
120 min
@Load 1.10 lb
ASTM D2471
 180 min
@Load 0.150 kg
180 min
@Load 0.331 lb
ASTM D2471
Working Life 300 - 360 min300 - 360 min
Shelf Life 18.0 Month18.0 Monthhardener
 36.0 Month36.0 Monthresin
 
Descriptive Properties
Mix ratio100:26.3--100:28.5Weight Range, Resin: Hardener
 100:27.0Weight, Resin: Hardener
 100:32.4–100:35.2Volume Range, Resin: Hardener
 100:33.3Volume, Resin: Hardener
 3.00:1Volume, Resin: Hardener
 3.08:-2.84:1Volume Range, Resin: Hardener
 3.70:1Weight, Resin: Hardener
 3.80:1-3.50:1Weight Range, Resin: Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOUGP944 / 290787

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.