MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC A50-XHS Bulk molding compound
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Description: BMC A50­XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in pre­weighted slugs. Due to the excellent flow and controlled reactivity, BMC A50­XHS is well suited for injection, transfer or compression molding. Typical applications are circuit breakers, lighting housings and structural parts.

Information provided by Bulk Molding Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.79 - 1.99 g/ccmolded
Linear Mold Shrinkage 0.0015 - 0.0025 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 30 - 40
Tensile Strength at Break 8300 - 10300 psi
Flexural Yield Strength 18.0 - 22.0 ksi
Flexural Modulus 1.70e+6 - 1.90e+6 psi
Compressive Strength 16800 - 20800 psi
Izod Impact, Notched 10.0 - 12.0 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 375 - 425 V/milShort Time
Arc Resistance >= 186 sec
Comparative Tracking Index <= 500 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Mold Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC A50-XHS-U Bulk molding compound
A. Schulman BMC A50-XHS High Strength Grade Molding Compound
A. Schulman BMC 1412 Flame and Track Resistant
A. Schulman BMC 300 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC 310 Cosmetic and Appliance Grade Compound

PBMC965 / 135937

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.