MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

CRP Technology Windform® FR2 Glass Filled Flame Retardant Composite Polyamide for Additive Manufacturing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Windform® FR2 is a white, halogen free polyamide based material and is not electrically conductive. Windform® FR2 combines outstanding wear resistance with good temperature resistance. It allows for good detail resolution with smoother surface finish when compared to Windform® FR1. It passed successfully the UL 94 HB 1 mm and 3 mm rating, the FAR 25.853 12-second vertical and 15-second horizontal flammability tests as well as the 45° Bunsen burner test and Smoke density test.

Applications: Owing to its flame-retardant quality and insulating properties, Windform® FR2 is suitable for Aircraft and Aerospace applications, Automotive parts (casings of electrical and electronic components, housing and enclosure assemblies), Consumer goods (lighting, appliances) and in general for any parts requiring flame retardancy.

Information provided by CRP Technology.

Key Words: Selective Laser Sintering (SLS)
Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878UNI EN ISO 868
Tensile Strength at Break 36.14 MPa5242 psiZ Axis; UNI EN ISO 527-1
 37.42 MPa5427 psiY Axis; UNI EN ISO 527-1
 44.36 MPa6434 psiX Axis; UNI EN ISO 527-1
Elongation at Break 2.68 %2.68 %Z Axis; UNI EN ISO 527-1
 2.78 %2.78 %X Axis; UNI EN ISO 527-1
 3.42 %3.42 %Y Axis; UNI EN ISO 527-1
Tensile Modulus 3.427 GPa497.1 ksiZ Axis; UNI EN ISO 527-1
 3.801 GPa551.3 ksiY Axis; UNI EN ISO 527-1
 4.608 GPa668.3 ksiX Axis; UNI EN ISO 527-1
Flexural Strength 76.52 MPa11100 psiUNI EN ISO 14125
Flexural Modulus 4.236 GPa614.4 ksiUNI EN ISO 14125
Poissons Ratio 0.280.28Z Axis; ASTM D638-14
 0.300.30Y Axis; ASTM D638-14
 0.390.39X Axis; ASTM D638-14
Charpy Impact Unnotched  1.56 J/cm²
@Temperature -40.0 °C
7.42 ft-lb/in²
@Temperature -40.0 °F
UNI EN ISO 179-1
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
UNI EN ISO 179-1
Charpy Impact, Notched  0.340 J/cm²
@Temperature -40.0 °C
1.62 ft-lb/in²
@Temperature -40.0 °F
UNI EN ISO 179-1
 0.440 J/cm²
@Temperature 23.0 °C
2.09 ft-lb/in²
@Temperature 73.4 °F
UNI EN ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.0e+10 ohm-cm8.0e+10 ohm-cmASTM D257-14
Surface Resistance 2.0e+12 ohm2.0e+12 ohmASTM D257-14
Comparative Tracking Index 300 V300 VIEC 60112 Solution A
 
Thermal PropertiesMetricEnglishComments
Melting Point 181.7 °C359.1 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 122.6 °C252.7 °FISO 75 Method A
Vicat Softening Point 178.0 °C352.4 °F10 N; ISO 306 Method A50
Flammability, UL94  HB
@Thickness 1.00 mm
HB
@Thickness 0.0394 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Smoke Density 4.0 min4.0 minPass, Flaming Mode; FAR/CS 25.853, Appendix F, Part V
 
Descriptive Properties
ColorOff White
Flammability - 12 seconds - VerticalPassFAR/CS 25.853 (a), Appendix F, Part I (a)(1)
Flammability - 15 seconds - HorizontalPassFAR/CS 25.853 (a), Appendix F, Part I (b)(5)
Flammability - 30 seconds - 45 degreePassFAR/CS 25.853 (a), Appendix F, Part I (b)(6)
Specific Flexural Modulus3131 MPa/(g/cc)Flexural Modulus per density unit
Specific Flexural Strength56.6 MPa/(g/cc)Flexural Strength per density unit
Specific Tensile Modulus3406MPa/(g/cc)Tensile Modulus per density unit
Specific Tensile Strength32.8 MPa/(g/cc)UTS per density unit
Surface Finish0.73 Ra µmAfter CNC machining
 1.68 Ra µmAfter Manual Finishing
 6.78 Ra µmAfter SLS Process

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRPT41t / 248982

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.