Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses: Cable Jacketing Wire Types: SEOW; SEW; SJEOW; SJEW; STEOW; STEW; VW-1 Agency Ratings: UL Class 11; UL Class 12; UL Class 36; UL Class 43; UL QMTM2 RoHS Compliance: RoHS Compliant Form: Pellets Information provided by Teknor Apex |