MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Controltac™ 8620 ES Conformable Graphic Film
Categories: Polymer; Film

Material Notes: These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making them perfect for signs and fleet graphics, including surfaces with corrugations and rivets. Use for electrostatic printing. Films 8620C, 8620Cv2 and 8620Cv3 with Comply adhesive have air release channels for fast and easy, bubble-free graphic installations. The air release channels for films with Comply v2 and Comply v3 adhesive are non-visible. The channels in 8620Cv3 also have improved air release.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milwithout adhesive
 3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 17.2 MPa
Peel Strength 3.50 pliAdhesion to Acrylic enamel
 4.00 pliAdhesion to Fruehauf pre-painted panels
 4.20 pliAdhesion to ABS
 4.80 pliAdhesion to Chrome
 5.20 pliAdhesion to Aluminum, etched
 7.90 pliAdhesion to Aluminum, anodized
 
Processing PropertiesOriginal ValueComments
Processing Temperature 4.00 - 38.0 °CApplication Temp; Flat surfaces without rivets
 16.0 - 32.0 °CApplication Temp; Compound curves
 10.0 - 38.0 °CApplication Temp; Curved or corrugated surfaces with rivets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 8620 Steel, direct quenched from pot, 230°C (450°F) temper, carburized
AISI 8620 Steel, mock carburized, reheated and oil quenched, 150°C (300°F) temper, 13 mm (0.5 in.) round
AISI 8620 Steel, mock carburized, reheated and oil quenched, 230°C (450°F) temper, 100 mm (4 in.) round
AISI 8620 Steel, normalized, 13 mm (0.5 in.) round
AISI 8620 Steel, normalized, 25 mm (1 in.) round

PMM34799 / 169546

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.