MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 1144 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Key Words: UNS G11410
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 217
Hardness, Knoop 240Converted from Brinell
Hardness, Rockwell B 95Converted from Brinell
Hardness, Rockwell C 17
Hardness, Vickers 228Converted from Brinell
Tensile Strength, Ultimate 745 MPa
Tensile Strength, Yield 620 MPa
Elongation at Break 10 %in 50 mm
Reduction of Area 30 %
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Typical For Steel
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000174 ohm-cmTypical steel
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.472 J/g-°CTypical steel
Thermal Conductivity 49.8 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 - 0.48 %
Iron, Fe 97.50 - 98.01 %As remainder
Manganese, Mn 1.35 - 1.65 %
Phosphorus, P <= 0.040 %
Sulfur, S 0.24 - 0.33 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1144 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1018 Steel, cold drawn
AK Steel ASTM A 1011, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS)
Aluminum 6061-T6; 6061-T651
ASTM A36 Steel, bar

M1144B / 7242

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.