MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AGC Asahiklin AE3100E Fluorinated Solvent
Categories: Fluid; Solvent

Material Notes: Asahiklin AE3100E is a fluorinated solvent used for cleaning, alcohol drying, and dewatering. This Hydrofluoroether (HFE-347pc-f) is a nonflammable solvent that has excellent material compatibility, low surface tension, low surface tension, low Global Warming Potential, and Zero ODP.

Applications:

  • Defluxing of electronics, electrical components, and printed wiring assemblies
  • Precision cleaning of metals, alloys, composites, and plastics
  • Drying agent after cleaning with hydrocarbons or alcohols
  • Drying after wet plating and for Carbide Metal before coating
  • Particle removal
  • Replacement for HCFC, Dupont™ Vetrel® & 3M™ Novec™ solvents
Benefits:
  • Non-flammable
  • Non-corrosive
  • Low global warming potential (GWP)
  • Zero ozone depletion potential (ODP)
  • Excellent thermal, chemical, and hydrolytic stability
  • Low surface tension, low viscosity, high liquid density
  • Superior drying property
  • Excellent permeability
  • Recyclable
  • Recoverable by simple distillation
  • Can be used with ultrasonics
  • No surfactants necessary

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/cc
Viscosity 0.602 cP
Vapor Pressure 0.271 atm
Surface Tension 16.1 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 187 J/g
@Temperature 51.0 °C
Specific Heat Capacity 1.49 J/g-°C
Melting Point -86.0 °C
Boiling Point 54.0 °C
 
Descriptive Properties
Global Warming Potential540
Material CompatibilityABSat boiling point for 3 days, <7.5% Weight change, <2.5% Linear Swell
 EPDMat boiling point for 3 days, <0.1% Weight change, <0.1% Linear Swell
 Fluoroelastomerat boiling point for 3 days, >69% Weight change, >21% Linear Swell
 Polymethyl methacrylateat boiling point for 3 days, affected weight change, affected linear swell
 Polypropyleneat boiling point for 3 days, <2.5% Weight change, <2.0% Linear Swell
 Polystyreneat boiling point for 3 days, <2% Weight change, <1% Linear Swell
 PTFEat boiling point for 3 days, <2.5% Weight change, <2.5% Linear Swell
 Silicon rubberat boiling point for 3 days, <20% Weight change, <5% Linear Swell
Material Composition3-8%Ethanol
 92-97%1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether
Relative Evaporation Rate66Ether=100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAGCX074 / 191183

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.