MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Permatex® Anaerobic Flange Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes: Permatex® Anaerobic Flange Sealant is a single component, medium strength, thixotropic, anaerobic sealant that cures rapidly. The product cures when confined in the absence of air between close fitting metal flanges. It provides a tough, resilient, solvent and temperature resistant seal that flexes with flange movement caused by vibration, pressurization or thermal changes.

The rate of cure will depend on the substrate used. The graph below shows the shear strength developed with time on grit blasted steel lap shears compared to different materials and tested according to ASTM D 1002. Where cure speed is unacceptably long, or large gaps are present, applying activator to the surface will improve cure speed. The graph below shows the shear strength developed with time using Surface Prep Activator on grit blasted steel lap shears and tested according to ASTM D 1002.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 275000 - 950000 cPThixotropic
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 200 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.250 - 2.00 hourPrimed
 1.00 - 12.0 hourUnprimed
 
Descriptive Properties
Chemical TypeMethacrylate Ester
Chemical/Solvent Resistance (%)100Motor Oil. 1000 hr @ 125°C.
 100Trans Fluid, 500 hrs, 23°C
 60Gasoline. 500 hr @ 23°C
 70Antifreeze. 500 hrs @ 87°C.
 90Heat Aged. 1000hrs @ 150°C.
ColorPurpleGel
Gap Filling (in)0.01diametral (Unprimed)
 0.05diametral (Primed)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWP9154 / 239664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.