MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Haysite H722 Polyester, Glass Reinforced
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: H722 is an all-purpose GPO-1 fiberglass mat reinforced thermoset polyester molded sheet. Available in thicknesses ranging from .031" - 2.00". Standard color - Natural. Meets Gov't Specs - LP-509, I-24768/6.

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.87 g/ccASTM D792
Water Absorption 0.60 %ASTM D229
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 46
Tensile Strength 10000 psiASTM D638
Flexural Strength 18000 psiASTM D790
Flexural Modulus 1.00e+6 psiASTM D790
Compressive Strength 32000 psiASTM D695
Shear Strength 14000 psiASTM D732
Adhesive Bond Strength 1250 psi
@Thickness 12.7 mm
ASTM D229
Izod Impact, Notched 8.00 ft-lb/inEdgewise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.3
@Frequency 1e+6 Hz
ASTM D150
 4.8
@Frequency 60 Hz
ASTM D150
Dielectric Strength 500 V/milPerpendicular, short time in oil; ASTM D149
Dielectric Breakdown 54000 VParallel, Step-By-Step in Oil; ASTM D149
Dissipation Factor 0.011
@Frequency 1e+6 Hz
ASTM D150
 0.015
@Frequency 60 Hz
ASTM D150
Arc Resistance 150 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Inert 130 °C
Flammability, UL94 HB
 
Descriptive Properties
Flame Resistance328 secondsBurning Time, ASTM D229
 57 secondsIgnition Time, ASTM D229

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)
Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3)
Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass

PHAY513 / 142469

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.