MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oceanchem Group Decabromodiphenyl Ethane (DBDPE/8010)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C14Br10H4

Cas No.: 84852-53-9

Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.

Use: This product is a new high efficiency, environmentally friendly flame retardant developed by our company and Beijing Institute of Technology. The product has properties of high bromine content, excellent thermal stability, low toxicity and UV-resistance. It is used in high-impact polystyrene, engineering plastics, wires and cables, insulator, elastomer and thermoset plastics etc.

Storage and Transportation: Handle with care, keep air-tight and dry.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.10 %
Brightness >= 85.0 %Grade I Whiteness
 >= 87.0 %Best Grade Whiteness
Particle Size <= 3.0 µmBest Grade
 <= 5.0 µmGrade I
Molecular Weight 971.22 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 340 °C
 
Component Elements PropertiesOriginal ValueComments
Bromine, Br 81.0 - 82.0 %
 
Descriptive Properties
CAS Number84852-53-9
Free Br (ppm)<10
Molecular FormulaC14Br10H4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy

POCEAN02 / 104206

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.