MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Struktol STRUKSILON 8030 Silicone Stabilizer for PU-Rigid Foam
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: STRUKSILON 8030 is a universal stabilizer for the production of polyurethane rigid foams. Due to its excellent flow properties and the very good insulation values that can be achieved STRUKSILON 8030 is especially recommended for 141 b blown formulation for appliance applications, pipe insulation and the production of PUR panels. Good results may also be achieved, when used in n-,i- or cyclopentane blown systems. For these formulations the system compatibility should be checked.

Applications:

Information provided by Struktol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.032 g/cc0.03728 lb/in³
Viscosity 950 cP
@Temperature 25.0 °C
950 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 100 °C>= 212 °FDIN/ISO 2562
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45
@Temperature 25.0 °C
1.45
@Temperature 77.0 °F
 
Descriptive Properties
AppearanceClear, colorless to slightly yellow liquid
Turbidity Point °C36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg AEM Eccofloat® TG-34/7000 Syntactic Foam
Novatec Novablend® 8888 PVC
Novatec Novablend® 8829 PVC
Northstar Polymers MPL-R20B Rigid Polyurethane Foam Formulation
Dow PAPI™ 20 Polymeric MDI

PSTRUK77 / 69304

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.