MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Methyl phenyl ether
Categories: Fluid; Solvent

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.996 g/cc
@Temperature 20.0 °C
0.0360 lb/in³
@Temperature 68.0 °F
Viscosity 1.359 cP
@Temperature 20.0 °C
1.359 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 108.14 g/mol108.14 g/mol
Vapor Pressure 0.003258 bar
@Temperature 20.0 °C
2.444 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 41.7 bar31300 torr
Critical Temperature 368 °C694 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point -37.5 °C-35.5 °F
Boiling Point 153.7 °C308.7 °F
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.2394
Antoine's Vapor Pressure B Parameter3430.82
Antoine's Vapor Pressure C Parameter-69.58
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
Critical Compressibility (Zc)0
Dipole moment (p/C.m)4.003E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A1316.4
Dynamic Viscosity Parameter B310.82
Molar Heat Capacity (298K)0 J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTOWAX® SH 105 Powder Paraffin Wax
Lithium Nitrate, LiNO3
Hong Kun Group UV 234 UV Absorber
Germanium, Ge
Evonik VESTOWAX® H 2050 SF Hard Paraffin Wax

VORGS235 / 99599

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.