MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hyosung Topilene HJ340 PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: Topilene ® HJ340 is a specially designed polypropylene block copolymer that features excellent stiffness & impact strength balance and enhanced thermal stability. It is suitable material for high stiffness sheets and industrial materials. Topilene® HJ340 complies with FDA requirements in the code of Federal Regulations in 21 CFR 177.1520 for food contact.

Typical Applications: Extrusion Molding: Corrugated sheets, High stiffness sheets Injection Molding: Industrial articles(Container, Crate, Pallet), Housewares, General goods

Features: Excellent stiffness & Impact strength balance / Enhanced thermal stability / Good processability in extrusion and injection molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Storage Temperature 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 80ASTM D785
Tensile Strength, Yield 300 kg(f)/cm²ASTM D638
Flexural Modulus 16000 kg(f)/cm²ASTM D790
Izod Impact, Notched 5.00 kg-cm/cm
@Temperature -10.0 °C
ASTM D256
Izod Impact, Unnotched 12.0 kg-cm/cmASTM D256
 
Processing PropertiesOriginal ValueComments
Drying Temperature 80.0 - 100 °C
Dry Time 2.00 - 4.00 hourair circulated condition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hyosung Topilene J340 PP
Hyosung Topilene HB240P PP
Hyosung Topilene B240T PP
Hyosung Topilene HJ740 PP
Hyosung Topilene HJ640A PP

PHYOS65 / 47951

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.