MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Proto3000 ABS-M30 Fused Deposition Modeling Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: Description: ABS-M30 is up to 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual modeling, functional prototyping, manufacturing tools, and end-use-parts. ABS-M30 has greater tensile, impact, and ?exural strength than standard ABS. Layer bonding is signi?cantly stronger than that of standard ABS, for a more durable part. This results in more realistic functional tests and higher quality parts for end use. When combined with a Fortus 3D Production System, ABS-M30 gives you Real Parts that are stronger, smoother, and with better feature detail.

Available Colors: Ivory, White, Black, Dark Grey, Red, and Blue

Information provided by Proto3000 for their protoyping engineering services.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109.5ASTM D785
Tensile Strength at Break 36.0 MPaType 1, 2"/min; ASTM D638
Elongation at Break 4.0 %ASTM D638
Tensile Modulus 2413 MPaASTM D638
Flexural Strength 61.0 MPaMethod 1, 0.05"/min; ASTM D790
Flexural Modulus 2317 MPaASTM D790
Izod Impact, Notched 139 J/mMethod A; ASTM D256
Izod Impact, Unnotched 2.83 J/cmMethod A; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 28.0 kV/mmIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 82.2 µm/m-°C
@Temperature -40.0 - 100 °C
ASTM E831
CTE, linear, Transverse to Flow 84.6 µm/m-°C
@Temperature -40.0 - 100 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
@Thickness 0.125 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
@Thickness 0.125 mm
unannealed; ASTM D648
Vicat Softening Point 99.0 °CRate B/50; ASTM D1525
Glass Transition Temp, Tg 108 °CDAM (SSYS)
Flammability, UL94 HB
@Thickness 0.850 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® ABS-M30
Proto3000 ABS-M30i Fused Deposition Modeling Polymer
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Stratasys® ABSi
Stratasys® PC Polycarbonate for 3D Printing

PPROTO969 / 133172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.