RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures up to 400°F. RM-3002 BMI delivers improved damage tolerance at higher temperatures vs. industry-standard BMI’s. Renegade precision-quality prepregs exhibit excellent handling characteristics and are available in woven and unidirectional form on various fibers including carbon, quartz and S2 glass. A wide variety of nano-materials can be incorporated into this resin system for tailored laminate properties and multi-functional performance. Renegade offers paste (RM-3006 and RM-3007) and film (RM-3011) adhesives compatible with RM-3002. Renegade also offers similar resin systems for RTM (RM-3000) or VARTM (RM-3010) processing. Typical properties. Tensile and flexural data has been normalized to 60% fiber volume. Information provided by Renegade Materials Corporation. Renegade Materials has been acquired by Teijin. |