MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Plastics TufFlex™ GTPO8290 Natural TPO Compound
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Application: An olefin based insulation & jacketing , 105°C rated compound formulated with excellent deformation characteristics. (SEW, SJEW)

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.850 - 0.910 g/cc0.850 - 0.910 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength >= 13.8 MPa>= 2000 psiASTM D638
Elongation at Yield >= 450 %>= 450 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.32.3ASTM D1531
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -55.0 °C-67.0 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adflex™ KS-021P TPO Resin
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO)
Teknor Apex Telcar® TL-2683D Thermoplastic Elastomer
Multibase Multi-Flex® TPO D 3218
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer

PSEPN030 / 179034

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.