MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm CYROLITE G-20 Acrylic-Based Multipolymer Molding Compound
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: CYROLITE G-20 compound is a impact-modified acrylic-based multipolymer for molding and extrusion of medical applications. Typical properties of CYROLITE G-20 compound are:
  • excellent chemical resistance to fats and oils
  • excellent bonding and welding capabilities
  • excellent bonding to PVC tubing
  • good impact strength
  • good light transmission
  • good heat resistance
  • good resistance to EtO, gamma and E-beam sterilization
Applications: Used for injection molding and extrusion of medical devices, medical packaging, as well as food packaging, toys and appliance parts.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccASTM D792
Water Absorption <= 0.30 %ASTM D570
Viscosity 975000 cP
@Shear Rate 100 1/s,
Temperature 240 °C
Approximate value
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D551
Melt Flow 2.2 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
Spiral Flow 46.0 cm215°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 39ASTM D785
Tensile Strength, Ultimate 47.0 MPaASTM D638
Elongation at Break 6.7 %ASTM D638
Elongation at Yield 4.0 %ASTM D638
Tensile Modulus 2.20 GPaASTM D638
Flexural Yield Strength 72.0 MPaASTM D790
Flexural Modulus 2.30 GPaASTM D790
Compressive Yield Strength 79.0 MPaASTM D695
Izod Impact, Notched 0.590 J/cm
@Thickness 6.35 mm,
Temperature 0.000 °C
bar; ASTM D256
 1.01 J/cm
@Diameter 6.35 mm
bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 92.5 µm/m-°C
@Temperature 0.000 - 100 °C
Specific Heat Capacity 1.30 J/g-°C
@Temperature 25.0 °C
 1.90 J/g-°C
@Temperature 100 °C
 2.30 J/g-°C
@Temperature 175 °C
Thermal Conductivity 0.220 W/m-K
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °CAnnealed; ASTM D648
Vicat Softening Point 101 °CASTM D1525
Flammability, UL94 HB
Oxygen Index 19 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.515ASTM D542
Haze 7.0 %ASTM D1003
Yellow Index -0.300 %
Transmission, Visible 90 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 216 - 249 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm CYROLITE G20-HIFLO Acrylic-Based Multipolymer Compound
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer

PCYR18 / 29157

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.