MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion AIF3 Aluminum Fluoride for Optical Coating
Categories: Ceramic; Halide

Material Notes: Fluoride compounds are used in coatings for the UV to middle-IR regions. They provide the lowest refractive indices and therefore are essential components of anti-reflective coatings. Fluoride films display absorption bands in the IR regions 2.8-3.2 µm and 6.0-7.4 µm to varying depths, depending on the compound and thedeposition method and parameters. High substrate temperatures, E-beam and IAD are methods that reduce the depths of the absorptions.

Aluminum Fluoride, AlF3, is a well-known material which has previously been used as a coating material where a low index was required. It is not affected by water and has good mechanical strength.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.90 g/ccCrystal
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 1260 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.30
@Wavelength 10000 nm
 1.30
@Wavelength 12000 nm
 1.31
@Wavelength 8000 nm
 1.32
@Wavelength 4000 nm
 1.34
@Wavelength 800 nm
 1.34
@Wavelength 1000 nm
 1.36
@Wavelength 600 nm
Transmission, Visible 92.0 %
@Thickness 0.0110 mm
8% Absorption
 96.0 %
@Thickness 0.0100 mm
4% Absorption
 98.0 %
@Thickness 0.00900 mm
2% Absorption
 >= 99.0 %
@Thickness 0.00800 mm
<1% Absorption
 100 %
@Thickness 0.000250 - 0.00100 mm
0% Adsorption
 
Descriptive Properties
ColorWhite
Evaporation Temperature<1100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMATER900 / 323494

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.