MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewable material as certified according to ASTM-D6866. The OnFlex™ BIO 5100 series compounds are formulated to provide excellent toughness, abrasion resistance and mechanical properties.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183
Filler Content 30 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ISO 868
Tensile Strength at Break 75.0 MPaISO 527-2
Elongation at Break 15 %ISO 527-2
Tensile Modulus 2500 MPaISO 527-2
Flexural Strength 64.0 MPaISO 178
Flexural Modulus 2280 MPaISO 178
Charpy Impact Unnotched 34.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 97.0 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 4.50 kJ/m²
@Temperature -30.0 °C
ISO 179
 18.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Processing PropertiesOriginal ValueComments
Melt Temperature 225 - 250 °C
Mold Temperature 30.0 - 60.0 °C
Drying Temperature 100 - 120 °C
Dry Time 1.00 - 2.00 hour
 
Descriptive Properties
Biobased Content30%ASTM D6866
FeaturesAblation Resistant
 Good Toughness
 Renewable Resource Content
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Injection RateSlow
Processing MethodInjection Molding
 Multi Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Consumer Applications
 General Purpose
 Sporting Goods

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE)
Avient OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE)

PH0POL1116 / 145685

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.